Hi
At the first,it is important that the mechanical properties of chosen
material be the same,
the yield point and the tensile point of A36 is the same for all
thicknesses, But there is a little difference about the material
(Specially sheet metal) that is categorized by EN 10025 like s235
becuase the yield point of the s235 that is similar to A36 (almost)
is going down when the thickness is going up but the issue that is
very important is the Design assumptions.
I can send you the summarized properties of the materials if you want
but the final decision must be taken by the designer and accorting to
design assumption.

regards
M.R

On Jan 31, 4:52 pm, Srinivas Engr <srinivas.gmsr...@gmail.com> wrote:
> Dear All.
> pl guide be about in selction of equivalent grade material?
> Wat we have to look?
> & In which spec we have to refer?
> Wat r A36 equivalent materials..?
> Wat about S275 grade material?
>
> Thanks & Regards
> Srinivas

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...