Friday, January 28, 2011

Re: [MW:9537] heat input calculation in welding

Hello Kumar,
You have to calculate the heat input for all the runs seperately, and the one with the highest heat input will be given consideration.
Note: you have to oberve you interpass temperature and other parameters during the test.
Regards
Paul osikwemhe.

On Fri, Jan 28, 2011 at 6:19 AM, sandy <kumar.sandeep@siemens.com> wrote:
Hi everybody

I have one query regarding the heat input.
If I am welding a joint with multipass, then I have diffrent heat
input for every pass depening on the parameters. now I want to know
which heat input shall be taken into consideration for the effect of
heat input on base metal, cauz every pass has its effect on base metal
and after every pass due to the previous heat input I am giving extra
heat in the base metal.
So I want to know should I take individual heat input or sum of all
heat input for getting the exact effect of Heat input on base metal.

Regards
Sandeep Kumar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...