Friday, January 28, 2011

Re: [MW:9539] Duplex stain less steel certificates misses nitrogen content

Replied below to yor queries.
Regards,
Ajay

From: murugesan jeyaraman <jmurugesan@gmail.com>
To: materials-welding@googlegroups.com
Sent: Fri, January 28, 2011 5:17:07 AM
Subject: [MW:9532] Duplex stain less steel certificates misses nitrogen content

Dear all
 
I reviewed a Material certificate for Duplex SS, Plate A240 UNS S31803 and found Nitrogen content .08 – 0.2% as required by ASME sec II part A is not at all mentioned in the certificate. As vessels are fabricated and welded I issued a NCR to manufacturer.

 

Vessel manufacturer are going to ask Mill about this.

 

1) My question is how come a Mill certificate misses an essential element of composition required by the code?  If the Mill comes with a reply that it is a clerical error to miss the Nitrogen content, and re-issue a certificate, can we accept it as genuine?

It may happen, sometimes the Mill misses to include such information. I believe, if the Mill re-issues the certificate afte correction, then you can accept it.

 

2) Is nitrogen content can be analysed by PMI or any other analyzing method in a lab test. Because the vessel fabricator say they are going to do lab test, for this.

The vessel manufacturer may have left over materials of same heat, which can be chemically tested at lab's for more perfect analysis or even by PMI as suggested by Mr. Karthik.

 

Please share your experiences and opinion about this.

 

Thanks

 

Murugesan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...