Dear Murugan,
 
I hope Mill always keeping all Batch / Heat Number materials  in stock with them in LAB / R&D Department. So, based on your request they will do the required test with you Heath Number materials.
 
 

On Fri, Jan 28, 2011 at 3:17 AM, murugesan jeyaraman <jmurugesan@gmail.com> wrote:
Dear all
 
I reviewed a Material certificate for Duplex SS, Plate A240 UNS S31803 and found Nitrogen content .08 – 0.2% as required by ASME sec II part A is not at all mentioned in the certificate. As vessels are fabricated and welded I issued a NCR to manufacturer.

 

Vessel manufacturer are going to ask Mill about this.

 

1) My question is how come a Mill certificate misses an essential element of composition required by the code?  If the Mill comes with a reply that it is a clerical error to miss the Nitrogen content, and re-issue a certificate, can we accept it as genuine?

 

2) Is nitrogen content can be analysed by PMI or any other analyzing method in a lab test. Because the vessel fabricator say they are going to do lab test, for this.

 

Please share your experiences and opinion about this.

 

Thanks

 

Murugesan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...