Hi
 
There is no expiry date for the consumables.
 
You can use the consumables , as long as the condition is good.
 
May be you need to get approvals for the batch's if the approval is expired for the concerned consumables lot
 
Thanks & Regards,
 
K. Babu

----- Original Message -----
From: Suresh
Sent: Monday, January 31, 2011 1:15 PM
Subject: Re: [MW:9575] Expiry period for SMAW consumable-reg

Hii
 
Generally Consumable expiry date is up to 2 monsoons,or Manufacturer should specify in Batch/Lot certificate .

On Mon, Jan 31, 2011 at 9:35 AM, Pandiaraj <pandi.kali@gmail.com> wrote:
Dear Experts,
    generally what is expiry period for SMAw consumables (Flux coated) dose ASME Sec II-C refers regarding this, if so please refer which class.in the consumable wraper only manufactured date is given but not the expiry date.

Thanks & Regards,

K.Pandiarajan.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks  & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...