Re: [MW:9585] Effect of Polarity Change in SMAW

Hi,
Before changing just go through the ASME secII Part C for SMAW of your
selected electrode and see the requirement of polarity and also go
through the manufacturers recommendation.


On Mon, 31 Jan 2011 13:20:23 +0530 wrote
>Dear All,
In SMAW process, generally the polarity is DCEP(Direct Current
Electrode Positive).I would like to get some advise on my following
queries.

1. Is there any problem, if I am changing the polarity to DCEN in SMAW
process?
2. Is this polarity change has any effect on metallurgical properties
of materials comes under carbon steel family?
3. Is this polarity change has any effect on metallurgical properties
of non ferrous materials?
 
Regards,
 
Limesh
 



--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
>


Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...