Monday, January 31, 2011

Re: [MW:9601] P1 no Range

Dear Puneet,
 
IS 2062 Gr A, is unlisted , but max. properties were equalent to P1. but while preparing WPS/PQR use Material Spec as IS 2062 GrA .
 
SS 410 is Martensitic Steels, its P No is 6

On Sun, Jan 30, 2011 at 8:04 PM, puneet takiar <puneet1takiar@yahoo.com> wrote:
Hello!
Can anybody tell me in which P. no IS 2062 grade A and SS 410 will fall and how to search in ASME sex IX table.
Regards, 

puneet takiar





From: Karthik <karthik6684@yahoo.com>
To: materials-welding@googlegroups.com
Sent: Fri, 7 January, 2011 1:46:08 PM
Subject: Re: [MW:0] P1 no Range

Hi,
Please refer QW423 also QW 350 for essential variables.

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Fri, 1/7/11, sn vl <weldinspn@gmail.com> wrote:

From: sn vl <weldinspn@gmail.com>
Subject: [MW:9122] P1 no Range
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Friday, January 7, 2011, 2:43 PM

Hi..

How to find in ASME sec IX P no to Pno qualification range.
Eg : If a welder qualified for P1to P1
what is the Range qualified As per Sec IX.
Where is given in CODE.


Regards
SN.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...