Thursday, January 27, 2011

Re: Re: [MW:9518] SAW filler for SA516 Gr70

Dear all,
 
The diffrence between EM12K & EM14K is in the content of carbon not in manganese  i thought that Mr.John Henning is correct.We are going to make the PQR with EM14 K
 
Thanks to all for valuable information
Regards
 
Rinshad A
 
On Tue, Jan 25, 2011 at 4:49 PM, muthu barathi <muthu_barathi@rediffmail.com> wrote:
ok what about suitable SAW welding electrode for welding API 5 L Grade
X 65 Is this suitable F7A5-EH 12K



On Tue, 25 Jan 2011 16:53:48 +0530 wrote

>F7A4 - EM12K it self sufficient. No need to go for High magnese EM
14K..
 

BR,
MSMS

On Sat, Jan 15, 2011 at 12:14 AM, rinshad abdul rahman
wrote:


Dear all,


Which is the suitable filler for SAW on SA 516 Gr70 (with PWHT) ?


EM12K or EM14K


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.






--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
>


Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...