Dear Ali,
 
Please refer the below for your query
 
Position:
 

QW-203 Limits of Qualified Positions for

Procedures

Unless specifically required otherwise by the welding

variables (QW-250), a qualification in any position qualifies

the procedure for all positions. The welding process

and electrodes must be suitable for use in the positions

permitted by the WPS. A welder or welding operator making

and passing the WPS qualification test is qualified for

the position tested. See QW-301.2.

 

Backing:

 
 

QW-251.1 Types of Variables for Welding

Procedure Specifications (WPS). These variables (listed

for each welding process in tables QW-252 through

QW-265) are subdivided into essential variables, supplementary

essential variables, and nonessential variables

(QW-401). The "Brief of Variables" listed in the tables

are for reference
only.

 

Date: Fri, 26 Apr 2013 11:27:25 +0400
From: mhaskar.aly@gmail.com
To: materials-welding@googlegroups.com
Subject: [MW:17560] Welding Position & Backing in PQR

Dear Friends,
Is welding position & backing is the criteria for PQR;
 
Can we  use any position , with or without backing for PQR...and we don't have any restriction on above parameters
 
 
 
Kindly clarify as per ASME SEc IX
 
Ali

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...